The industrial application of Polymer Inclusion Membranes (PIMs) for pharmaceutical wastewater remediation is often limited by the extraction–stripping trade-off and carrier-mediated transport kine...
<p><strong>Tác giả:</strong> Ebenezer Idowu Oluwasola, Sunday Joseph Olusegun, Ewa Felis</p>
<p>The industrial application of Polymer Inclusion Membranes (PIMs) for pharmaceutical wastewater remediation is often limited by the extraction–stripping trade-off and carrier-mediated transport kinetics. To bypass these limitations, this study introduces a highly efficient, liquid-plasticizer-free, self-plasticizing bi-continuous network PIM system and employs a 1 M NaCl strip phase. This transition provides mobile chloride (Cl⁻) counter-ions that trigger an accelerated, continuous ion-exchang...</p>
<p>📄 DOI: <a href="https://doi.org/https://doi.org/10.1007/s11356-026-38333-3" target="_blank" rel="noopener">https://doi.org/10.1007/s11356-026-38333-3</a></p>
<p>📖 <a href="https://doi.org/https://doi.org/10.1007/s11356-026-38333-3" target="_blank" rel="noopener">Xem bài báo đầy đủ</a></p>
Bài viết được biên soạn lại bởi LIFVietnam. Nguồn tham khảo: OpenAlex